FM-4411 | Reactive PDMS - Bi terminal Hydroxy

Harmonization Code : 3910.00.00.60 | Polydimethylsiloxane, whether or not polyethylene glycol and trifluoropropyl substituted, with methacrylate end groups

FM-4411 | Reactive PDMS - Bi terminal Hydroxy

Main features

  • Bi terminal
  • 1,000 g/mol | 35 mPas
  • Hydroxy functional groups

Product Description

Silaplane® FM-4411 is a reactive polydimethylsiloxane (PDMS) based polymer with a molecular weight of 1,000 g/mol and a Viscosity of 30 - 40 mPas. This reactive silicone material offers the addition of silicone-type properties to non-Silicone materials in a variety of industries including electronics, semiconductors, automotive, biotech, healthcare, and clean energy applications. It offers narrow polydispersity and a low level of chemical impurities.

Silaplane® FM-4411 bi-terminal product has two Hydroxy functional groups that are reactive toward a variety of compounds and surfaces enabling chemical and physical changes to chemicals, particle surfaces and larger surface structures. Hydroxy groups are mainly reactive with urethane and ester compounds.

Product Family

FM-4411/1KC

1kg can
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Can
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 11 x 11 x 16.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Molecular weight
1000 g/mol
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.97
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
35 mPa.s