Hysol MG57F-0660 | Gold Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

MG57F-0660 Gold Epoxy Mold Compound Hysol MG57F-0660 | Gold Epoxy Mold Compound

Main features

  • Gold epoxy mold compound
  • Laser Markable
  • Designed for MnO2 Tantalum Capacitors

Product Description

Hysol MG57F-0660 is a gold-colored, environmentally friendly “green” (no bromine/antimony or phosphorous) molding compound. It has been designed especially for use in high volume molding of Manganese Oxide MnO2 tantalum capacitors. It offers excellent moldability with faster cycle times than most traditional epoxy based encapsulants and is especially recommended for automold applications.

Hysol MG57F-0660 also offers excellent contrast with currently available laser marking equipment making it ideal for laser marking product information on the component.

Curing Time

  • 20 to 35 seconds @170°C
  • 30 to 60 seconds @150°C

Post Cure

  • 2 hours @150°C

 

Product Family

MG57F-0660/40M40G15K

Pelletized - 40MM x 40GR | 15kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 15.51 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Gold
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.82
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
168 °C
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
35000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.42 %
Curing Conditions
Transfer Pressure
40 - 100 kg/cm2
Transfer Time
5 - 30 s

Additional Information

{tab=Applications}

Short Description of {product_name}

Typical applications and uses of {product_name} include:

  • MnO2 Tantlaum Capacitors
  • Other tantalum capacitor packages

Technical Datasheets for {product_name}

TDS (English) Kapton_Technical_Data_Sheet Click to access {product_name} Technical Data Sheet
*Note that only registered users may access technical datasheets

{tab=Packaging Details}

Packaging Details for {product_name}

The following information is specifically related to each unit of measure of {product_name}. If you which to compare this to other product sizes, click on the respective product from the list above and check here for values specific to that product. These values are taken from our internal database and are used in the calculation of the gross weight and packaging dimensions of the goods during shipping. You can use these values to approximate delivery charges using your own carrier.

{/tabs}

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers