Hysol MG40FS | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

MG40FS PDIP Epoxy Mold Compound Duroplast Hysol MG40FS | Black Epoxy Mold Compound MG40FS PDIP Epoxy Mold Compound Duroplast

Main features

  • Designed for PDIP packages
  • Excellent HTRB performance
  • Ideal for high voltage discrete semiconductors

Product Description

Hysol MG40FS is a high productivity molding compound designed specifically for high volume encapsulation of PDIP, SOIC, Power discrete and High Voltage devices. This material is applicable for devices having chip dimensions up to 150 mils square. It has been formulated to provide the best possible moldability and as wide molding latitude as possible

Hysol MG40FS has excellent high temperature electrical stability. This makes it ideal for PDIP, TO220, TO247 and high voltage discrete semiconductor packages that need to resist higher temperatures. This product is available in both conventional (MG40FS) and automold (MG40FS-AM) versions.

Product Family

MG40FS/48M128G15K

Pelletized - 48MM x 128GR | 15kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 15.51 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.84
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
10000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.85 %
Physical Properties
Spiral Flow @ 175°C
89 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
160 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.95 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Mechanical Properties
Molded Shrinkage
0.5 %
Curing Conditions
Transfer Pressure
40 - 100 kg/cm2
Transfer Time
15 - 25 s

Additional Information

This product is not recommended for use in pure oxygen and/or oxygen rich systems and should not be selected as a sealant for chlorine or other strong oxidizing materials.