Hysol MG15F-0140 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Hysol MG15F-0140 | Black Epoxy Mold Compound

Main features

  • Anhydride cured
  • Tg: 195°C
  • For power discretes and high voltage rectifiers

Product Description

Hysol MG15F-0140 is a black, semiconductor grade, anhydride curing epoxy molding compound designed for high voltage power applications requiring good electrical stability at high temperature. A real classic. The work horse, as the industry would call it, product of the halogen and anhydride containing chemistries.

Hysol MG15F-0140 was typically used for power discretes and high voltage rectifiers. Despite its glorious history, the industry has been leaning towards next generation compounds that are future proof while still maintaining the same, or sometimes even better mold properties. GR 750 and the GR 750 XX series in general have nothing to envy and are good drop in candidates for the old guard.

 

MG15F-0140 will be discontinued by end of this year since its flame retardant (Dechlorane Plus) will be banned by the Chinese government by 2024. MG15F-0140 will be replaced with MG15F-0140B.
Product Family

MG15F-0140/P1K

Powder | 1kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 20 x 25 x 25 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
69 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.81
Chemical Properties
Moisture absorption
0.65 %
Physical Properties
Spiral Flow @ 175°C
50.8 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
195 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.66 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
63000000000000000 Ohms⋅cm
Curing Conditions
Transfer Time
6 - 15 s

Additional Information

Property Comparison Table of Hysol MG 15F-0140B vs Hysol MG15F-0140 

Property Unit MG 15F-0140B MG15F-0140
Gel time at 175°C s 18 17
Spiral flow at 175°C cm 56 56
Filler content % - 69
Shelf life at 5°C days 365 365
Preheat temperature (conventional mold) °C 77 to 94 75 to 95
Molding temperature °C 177 to 200 175 to 200
Molding pressure kgf/cm² 42 to 84 42 to 84
Transfer time s 6 to 15 6 to 15
Curing time (3 mm) at 177°C s 60 to 75 60 to 75
Curing time (3 mm) at 190°C s 45 to 60 45 to 60
Post cure time at 175°C h 8 to 12 8 to 12
Post cure time at 190°C h 2 to 4 2 to 6
Glass transition temperature (Tg) °C 185 195
CTE (alpha 1) below Tg ppm/°C 22 21
CTE (alpha 2) above Tg ppm/°C 57 70
Specific gravity - 1.81 1.81
Molded shrinkage % 0.34 0.2
Flexural strength MPa 115 127.5
Flexural modulus GPa 10.3 13.7
Thermal conductivity W/m-K - 0.65
Moisture absorption at 85°C/85% RH, 168 h % - 0.5
Volume resistivity at 500 V @ 21°C ohm-cm 4.3 × 1016 3.0 × 1016
Extractable ionic content: Chloride (Cl-) ppm 9.9 -
Extractable ionic content: Sodium (Na+) ppm 5 -
Water extract conductivity micromhos - 3
pH of extract - - 5.4
Flammability rating at 3 mm UL-94 V-0 V-0

Notes: Values are typical and should be confirmed against the latest product TDS and your process conditions. "-" indicates not yet available

This table summarizes and compares typical processing and cured-performance properties for two anhydride-cured epoxy molding compounds used in high-voltage power applications, showing that the molding window and cure conditions are broadly similar (gel time, spiral flow, transfer time, and cure schedules), while key material differences appear in thermo-mechanical and moisture-related behavior: MG15F-0140B reports lower Tg (195°C vs 185°C), lower CTE above Tg (70 vs 57 ppm/°C), lower flexural modulus (13.7 vs 10.3 GPa), but higher molded shrinkage (0.2% vs 0.34%), while both grades meet UL-94 V-0 at 3 mm and show high volume resistivity at 500 V and 21°C. 

 

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers