Hysol KL-G200S | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

KL-G200S Black Epoxy Mold Compound for SMX mini-pellets Hysol KL-G200S | Black Epoxy Mold Compound KL-G200S Black Epoxy Mold Compound for SMX mini-pellets

Main features

  • MSL 1 260°C
  • Low Cost of Ownership for Halogen free
  • Designed for DO214 (SMA, SMB & SMX) packages

Product Description

Hysol KL-G200S is a black, halogen-free, semiconductor grade epoxy molding compound. It provides the lowest cost of ownership for a "non-halogen containing" epoxy molding compound. It works on surface mounted diodes such as D0214 in various sizes (SMA, SMB, SMC) and other low end discrete semiconductor and sensor packages. 

Hysol KL-G200S passes MSL1 260°C. It is an epoxy molding compound that contains no bromine, antimony or phosphorus flame retardant. This product is designed to achieve JEDEC Level 1 requirements, at 260°C reflow temperature and provides the lowest cost of ownership with superior moldability and reliability. To top this up, it meets UL 94 V-0 Flammability at 6.35mm thickness.

Product Family

KL-G200S/C63K21

Pelletized - 35MM x 21GR | 15kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 15.51 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
77 %
Filler Size Cut
75 µm
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.95
Chemical Properties
Moisture absorption
0.5 %
Physical Properties
Spiral Flow @ 175°C
80 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
175 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1.4 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
18000000000000000 Ohms⋅cm
Mechanical Properties
Molded Shrinkage
0.26 %
Curing Conditions
Transfer Pressure
40 - 100 kg/cm2
Transfer Time
10 - 20 s