Hysol KL-G100S | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Hysol KL-G100S | Black Epoxy Mold Compound

Main features

  • Low CTE (13 ppm/°C)
  • Low stress
  • For SOD, MBF, ABS packages

Product Description

Hysol KL-G100S is a black, semiconductor grade, high productivity molding compound, providing a wide operation window. It is 80% filled with spherical/fused silica and achieves a flammability rating of V0 at UL94 testing conditions.

Hysol KL-G100S is an environmentally friendly molding compound with high moldability that has a low coefficient of thermal expansion (13ppm/°C). It is typically used for SOD, MBF and ABS semiconductor packages. Its CTI, comparative tracking index value is 525V.

Product Family

KL-G100S/14M7.5G1K

Pelletized - 14MM x 7.5GR | 1kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 1 kg
Gross weight 1.2 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
80 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.89
Chemical Properties
Moisture absorption
0.40 %
Physical Properties
Spiral Flow @ 175°C
91.4 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
153 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.74-1.07 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Mechanical Properties
Molded Shrinkage
0.25 %
Curing Conditions
Transfer Pressure
40 - 70 kg/cm2
Transfer Time
10 - 25 s

Additional Information

Additional Technical Information

Property Unit Temperature
25℃ 150℃ 175℃
Chlorine (Cl⁻) ppm 15
Sodium (Na⁺) ppm 4
Potassium (K⁺) ppm 1
Bromine (Br⁻) ppm 0
Sulfate (SO₄²⁻) ppm 1
Electrical Conductivity (oEW)
uS/cm 20 - -
Flexural Strength MPa 145 91 61
Flexural Modulus MPa 12,577 612 501
Adhesion Strength to Cu (Post-PMC)
MPa 0.90 1.14 1.02
Adhesion Strength to Cu (Post-MSL3)
MPa 0.40 0.17 0.12

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers