Hysol GR920 | Epoxy mold underfill

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR920 | Epoxy mold underfill

Main features

  • Molding underfill
  • Excellent narrow gap fill
  • Outstanding warpage control

Product Description

Hysol GR920 is a molding underfill product series. This product is not formulated with low-alpha silica but we could develop a low alpha version, suitable for memory chips, if needed.
 
Hysol GR920 is based on a MAR/LMW chemistry with an MF/MAR hardener and an MH flame retardant. Molding underfills are typically used for BGA, flip chip applications.
 
 
Features
  • Good reliability performance on advanced packaging
  • Excellent narrow space filling.
  • Meet MSL3~MSL2/260C requirement.
  • Outstanding warpage control(unit warpage<80 μm ).
  • Meet UL94 V-0 flammability rate at 1/8 inch thickness.

Available Version

  • Hysol GR920 H
  • Hysol GR920 Q
  • Hysol GR920 M
  • Hysol GR920 L
  • Hysol GR920 A

 

 

Product Family

GR920/14M4.4G10K

Pelletized - 14MM X 4.4GR | 10kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 10.51 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
2 g/cm3
Filler Content
88,5 %
Physical Properties
Spiral Flow @ 175°C
102 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
120 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.9 W/m.K
Mechanical Properties
Molded Shrinkage
0,17 %

Additional Information

GR920 Series Products Properties Comparison

Property / Product Unit  Hysol GR920 H Hysol GR920 Q Hysol GR920 M Hysol GR920 L Hysol GR920 A
UNCURED PROPERTIES
Packages - FCLGA FCCSP/FCLGA FCCSP FCBGA FCCSP
Filler cut µm 20 20 20 20 20
Filler content % 84 85 88.5 88 87.5
Filler Type   Spherical Spherical Spherical Spherical Spherical
Hot Plate Gel time, @ 175°C s 38 39 37 34 46
Spiral Flow @ 175°C inch 60 56 39 36 66
Halogen-free (Green)   ✔ ✔ ✔ ✔ ✔
TYPICAL CURED PROPERTIES
Glass Transition Temperature °C 102 138 120 158 150
Coefficient of Thermal Expansion (CTE) α1, TMA ppm/°C 13 12 10 9 9
Coefficient of Thermal Expansion (CTE) α2, TMA ppm/°C 45 45 35 33 34
Flexural Strength @25°C MPa 125 146 120 154 138
Flexural Modulus @25°C MPa 13500 15500 19500 17800 21000
Water Absorption, 24hr PCT % 0.4 0.35 0.3 0.3 0.38
Mold Shrinkage after PMC % 0.36 0.26 0.13 0.20 0.19
Specific Gravity - 1.93 1.96 1.99 1.99 1.98
Cl Content ppm 7 7 8 7 9
pH - 4.5 5.1 6.5 6.1 6.3
Moisture Sensitivity Level - 2 3 3 3 3
Feature -

Good Flowability 

Low Modulus

Good Flowability 

Low Modulus

Medium Tg

Low Modulus

Low Shrinkage

Low CTE

High Tg

Low Shrinkage

Low CTE

Good Flowability 

High Tg

Low Shrinkage

Low CTE

 

Beta Site Performance in HT**

Property / Product Unit  Commercial Hysol GR910 L20
UNCURED PROPERTIES
Epoxy Type   - MAR/MF
Hardener Type   - MAR/MF
Filler cut µm 20 20
Filler content % 88 88
Hot Plate Gel time, @ 175°C s 30 34
Spiral Flow @ 175°C cm 99 91
TYPICAL CURED PROPERTIES
Glass Transition Temperature, TMA °C 142 158
Glass Transition Temperature, DMA °C 150 156
Coefficient of Thermal Expansion (CTE) α1, TMA ppm/°C 9 9
Coefficient of Thermal Expansion (CTE) α2, TMA ppm/°C 37 33
Flexural Strength @25°C MPa 175 154
Flexural Modulus @25°C MPa 19500 17800
 Storage Modulus by DMA @25°C Mpa 25000 25914
 Storage Modulus by DMA @175°C Mpa 3000 2119
 Storage Modulus by DMA @260°C Mpa 1200 1203
Water Absorption, 24hr PCT % 0.38 0.37
Mold Shrinkage after PMC % 0.18 0.20
Hardness Shore D 83 81

 

Package Mold Cap Strip Size Package Size Die Size Bump Height
FCCSP 0.4 mm 240.5 * 95 * 0.22 mm 5.4 * 5.4 mm 3.3 * 2.8 * 0.15 mm 65 µm
 
Item Hysol GR910 L20
Appearance
C-Scan
T-Scan
Bump-Scan
Warpage

Short Side 2.07 mm

Long Side 2.11 mm

Marking OK
Test Item Qualification Test Condition Test Results Test Criterion SAT
Before Test / Pass NA
Pre-conditioning


Baking: 125°C, 24 hours

Moisture Soak: 30°C/60%RH, 192 hours

Reflow @ 260°C * 3times

Pass J-STD-020E
uHAST

130°C, 85%RH

33.3 psia, unbiased 192 hours

Pass JESD22-A118B
TCB -55°C~125°C, 1000 cycles Pass JESD22-A104E

 

Beta Site Performance in JT**

Property / Product Unit  Commercial Hysol GR910 L20
UNCURED PROPERTIES
Epoxy Type   - MAR/MF
Hardener Type   - MAR/MF
Filler cut µm 20 20
Filler content % 88 88
Hot Plate Gel time, @ 175°C s 30 34
Spiral Flow @ 175°C cm 99 91
TYPICAL CURED PROPERTIES
Glass Transition Temperature, TMA °C 142 158
Glass Transition Temperature, DMA °C 150 156
Coefficient of Thermal Expansion (CTE) α1, TMA ppm/°C 9 9
Coefficient of Thermal Expansion (CTE) α2, TMA ppm/°C 37 33
Flexural Strength @25°C MPa 175 154
Flexural Modulus @25°C MPa 19500 17800
 Storage Modulus by DMA @25°C Mpa 25000 25914
 Storage Modulus by DMA @175°C Mpa 3000 2119
 Storage Modulus by DMA @260°C Mpa 1200 1203
Water Absorption, 24hr PCT % 0.38 0.37
Mold Shrinkage after PMC % 0.18 0.20
Hardness Shore D 83 81

 

 

Package Mold Cap Strip Size Package Size Die Size Bump Height
FCCSP 0.365mm 240 * 95 * 0.18 mm 6.3 * 6.9 mm 6.35 *5.57 *0.15 mm 80 µm
 
Item Hysol GR910 L20
Appearance
C-Scan
T-Scan
Strip Warpage

2~3 mm

Marking OK
Test Item Qualification Test Condition Test Results Test Criterion
Before Test / Pass NA
Pre-conditioning


Baking: 125°C, 24 hours

Moisture Soak: 30°C/60%RH, 192 hours

Reflow @ 260°C * 3times

Pass J-STD-020E
uHAST

130°C, 85%RH

33.3 psia, unbiased 192 hours

Pass JESD22-A118B

 

Beta Site Performance in HJ**

Property / Product Unit  Commercial Hysol GR920 A1
UNCURED PROPERTIES
Epoxy Type   - BP
Hardener Type   - PN/MF
Filler cut µm 20 20
Filler content % 88 87.5
Hot Plate Gel time, @ 175°C s 30 46
Spiral Flow @ 175°C cm 99 167
TYPICAL CURED PROPERTIES
Glass Transition Temperature, TMA °C 142 150
Glass Transition Temperature, DMA °C 150 151
Coefficient of Thermal Expansion (CTE) α1, TMA ppm/°C 9 9
Coefficient of Thermal Expansion (CTE) α2, TMA ppm/°C 37 34
Flexural Strength @25°C MPa 175 1138
Flexural Modulus @25°C MPa 19500 21000
 Storage Modulus by DMA @25°C Mpa 25000 24000
 Storage Modulus by DMA @175°C Mpa 3000 2000
 Storage Modulus by DMA @260°C Mpa 1200 1100
Water Absorption, 24hr PCT % 0.38 0.38
Mold Shrinkage after PMC % 0.18 0.19
Hardness Shore D 83 80

 

 

Package Mold Cap Strip Size Package Size Die Size Bump Height
FCCSP 0.37 mm 240 * 76.3 * 0.18 mm 14 * 14 mm  6 * 6* 0.12mm 80 µm
 
Item Hysol GR910 L20
Appearance
C-Scan
T-Scan
Strip Warpage

2 mm

Marking OK
Test Item Qualification Test Condition Test Results Test Criterion
Before Test / Pass NA
Pre-conditioning


Baking: 125°C, 24 hours

Moisture Soak: 30°C/60%RH, 192 hours

Reflow @ 260°C * 3times

Pass J-STD-020E
uHAST

130°C, 85%RH

33.3 psia, unbiased 192 hours

Pass JESD22-A118B
TCB -55°C~125°C, 1000 cycles Pass JESD22-A104E

 

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers