Hysol GR910-K | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR910-K | Black Epoxy Mold Compound

Main features

  • Halogen free
  • High fluidity to avoid W/S issue
  • Designed for BGA/LGA

Product Description

Hysol GR910 K is a black epoxy molding compound specifically designed for Memory Ball Grid Arrays (BGA) and Land Grid Arrays (LGA). This semiconductor-grade material features spherical silica filler with a cut size of 53 µm, delivering exceptional fluidity and low shrinkage, which aids in advanced warpage control during manufacturing.

Hysol GR910 K is halogen-free and environmentally friendly, ensuring compliance with stringent safety standards. It offers excellent electrical performance, meeting the UL 94 V-0 flammability standard at a thickness of 1/8 inch.

Available Versions:

  • GR910 K | Optimized for high Tg and low modulus applications
  • GR910 K-31 | Tailored for high Tg and low shrinkage requirements

Key Features:

  • High Thermal Stability | Glass transition temperatures of 155°C (GR910 K) and 153°C (GR910 K-31)
  • Excellent Flowability | Ensures uniform coverage and filling during the molding process
  • Low Mold Shrinkage | 0.22% for GR910 K and 0.19% for GR910 K-31, contributing to precise dimensions
  • Low Coefficient of Thermal Expansion (CTE) | Minimizing stress during thermal cycling
  • Low Water Absorption | Less than 0.35%, enhancing reliability in humid environments

Highly Recommended For:

  • Advanced semiconductor packaging in high-performance applications
  • Memory devices requiring robust mechanical and thermal properties
  • Environmentally conscious projects where halogen-free materials are a must
Product Family

GR910K/14M4.4G15K

Pelletized - 14MM X 4.4GR | 15kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 15.5 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
86.5 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.97
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
155 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.9 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
40E15 Ohms⋅cm
Chemical Properties
Moisture absorption
0.35 %
Curing Conditions
Transfer Pressure
40 – 85 kg/cm2
Transfer Time
8 – 15 s
Physical Properties
Spiral Flow @ 175°C
200 cm

Additional Information

 
 GR910-K Series Product Properties Comparison
 
PROPERTY UNIT GR910 K GR910 K-31
Filler Content  % 86.5 89
Filler Cut um 53 53
Filler Shape - Spherical Spherical
Specific Gravity - 1.97 2.01
Spiral Flow  cm 200 172
Hot Plate Gel Time  sec 43 49
Glass Transition Temperature °C 155 153

CTE by TMA, α1

CTE by TMA, α2

ppm

ppm

10

37

9

32

Water Absorption (PCT24h)

wt%

0.35

0.33

Flexural Strength @25°C

Flexural Modulus @25°C

MPa

Gpa

141

19.8

145

24.5

Mold Shrinkage (After PMC)

%

0.22

0.19

Cl-

ppm 7 10
pH - 6.1 6.0
MSL Capability - MSL 2 MSL 3
Feature  

High Tg

Good Flowability

Low Modulus

High Tg

Low Shrinkage

Low CTE

 

Leading Brands Trust in Our Products and Services