Hysol GR900 Q1G2 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR900 Q1G2 | Black Epoxy Mold Compound

Main features

  • Designed for DFN and small QFN packages
  • Excellent electrical capabilities
  • Compatible with Copper Wire

Product Description

Hysol GR900 Q1G2 is a similar but alternative version of Q1L4. While Q1L4 offers great HTRB performance, Q1G2 offers better electrical performance for DFNs and small QFNs. It is a black semiconductor-grade epoxy molding compound designed for the encapsulation and protection of quad-flat no-leads (QFN) and dual-flat no-leads (DFN).

Hysol GR900 Q1G2 is a relatively softer, spherical silica filled (89%) high end epoxy, typically used for QFN and DFN packages. QFN and DFN packages are low-profile packages that are MAP molded. This means that the packages are molded together in one large mold and then separated by cutting through the entire package. Epoxy molding compounds made for these type packages, like Q1G2, must have a low warpage.

Hysol GR900 Q1G2 is an environmentally "green" halogen free product, meaning that it doesn't contain any bromine, antimony or phosphorus flame retardants. It offers good adhesion after MSL 3 and meets UL 94 V-0 Flammability at 1/8 inch (3.18mm) thickness. If you are not after the electrical performance, then by all accounts GR 900 Q1L4 will probably be the better option.

Product Family

GR900Q1G2/55M85.9G1K

Pelletized - 55MM x 85.9GR |1kg
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 30 x 30 x 30 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
89 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
112 °C
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Physical Properties
Spiral Flow @ 175°C
137 cm
Mechanical Properties
Molded Shrinkage
0.19 %
Curing Conditions
Transfer Pressure
40 - 100 kg/cm2
Transfer Time
5 - 30 s

Additional Information

 