Hysol GR730HT| Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR730HT| Black Epoxy Mold Compound

Main features

  • Halogen free
  • High adhesion
  • High thermal conductivity

Product Description

Hysol GR730HT is a halogen free, black, silica filled (90% filler weight) semiconductor grade epoxy molding compound designed for Power Supply in Package (PSIP). This low stress, low moisture absorption product is a commercial success with many uses on TO applications.

Hysol GR730HT is a black, heat curable epoxy molding compound that can be used in semiconductor packages such as TO252. Furthermore, it meets UL 94 V-0 flammability at 1/8 inch thickness.

Product Family

GR730HT/16M7.6G10K

Pelletized - 16MM X 7.6GR | 10kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 11 kg
Dimensions 26 x 28 x 25.5 cm

Technical Specifications

General Properties
Color
The color
Black
Filler Content
90 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.84
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
8000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.24 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
200 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.2 W/m.K
Physical Properties
Spiral Flow @ 175°C
76 cm

Additional Information

 

Property GR730HT (86W9HT) GR730HT (96G18) XX-G1250S X5HT XX-G3000HT
Filler content 90 90 86 87
Epoxy Modified Multi
functional type
Hydrophobic EP Modified Multi
functional type
Hydrophobic EP
Spiral Flow (inch) 76 86 120 120
Gel time (s) 20 30 30 35
Viscosity (PaS) 12 10 15 8
Specific Gravity 2.84 2.67 2.93 2.85
CTE 1 13 13 14 15
CTE 2 50 40 48 50
Tg (°C) 200 122 215 130
Flexural Strength/Modulus, Mpa 104/ 23000 122/ 24000 143/ 29000 180/ 25000
Mold Shrinkage (%) 0.14 0.25 0.12 0.33
Moisture Absorption PCT 0.24 0.24 0.45 0.35
Volume Resistance (@ 150) NA NA 5E12 5E12
Volume Resistance (@ RT) 8E15 7E15 NA NA
Impurity CI- 9 9 9 8
Thermal conductivity (W/mK) 3.2 3 2.9 3