Main features

  • High reliability
  • Green and halogen-free
  • Designed for SOT applications

Product Description

Hysol GR720 is a green, halogen-free epoxy molding compound specifically developed for SOT (Small Outline Transistor) packages with stringent requirements. GR720 sets new standards for performance and reliability in the electronics manufacturing realm. With a strong focus on die attach paste bonded SOT, GR720 excels in minimizing stress during bonding, ensuring the longevity of sensitive semiconductor components. Its low-stress formulation is a vital attribute, enhancing the durability of electronic devices.

Hysol GR720 its exceptional resistance to delamination, even after exposure to the rigorous conditions of MSL1 (Moisture Sensitivity Level 1) and TC1000 (Thermal Cycling at 1000 cycles). This outstanding performance guarantees the reliability of your devices, even when subjected to harsh environmental conditions. Moreover, Hysol GR720 offers exceptional workability, streamlining manufacturing operations and boosting overall efficiency.

Previously, packages molded with Hysol GR720 was able to achieve a Moisture Sensitivity Level (MSL) rating of 3 for die attach paste bonding. Additionally, it boasts remarkable filler properties with a filler content and cut of 84±1% and 75 µm, providing the best possible moldability and as wide a molding latitude as possible. HYSOL GR720 also meets UL94 V-0 Flammability at 1/8 inch thickness.

Product Family

GR720/11M3.5G15K

Pelletized - 11MM x 3.5GR | 15kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 16.5 kg
Dimensions 26 x 28 x 25.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
84 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.92
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
113 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.92 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V-0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
26×10¹⁵ Ohms⋅cm
Chemical Properties
Moisture absorption
0.40 %
Physical Properties
Spiral Flow @ 175°C
119.38 cm
Curing Conditions
Transfer Pressure
40–85 kg/cm2
Transfer Time
7–15 s

Additional Information

Adhesion Strenght Data

Property Value Unit
Adhesion at RT to Cu Substrate after PMC  7.22 MPa
Adhesion at RT to Cu Substrate after Preconditioning 

6.82

MPa

 

Storage

Keep the product in its sealed container within a dry environment. Material that has been taken out of its containers can become contaminated while in use. Please refrain from putting the product back into the original container.

Optimal Storage: 5 °C. Storage greater than 5°C can adversely affect product properties.