Hysol GR600 SL2| Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR600 SL2| Black Epoxy Mold Compound

Main features

  • High reliability
  • High power applications
  • Good electrical performance

Product Description

Hysol GR600 SL2 is a halogen free, black, silica filled (87% filler weight) semiconductor grade epoxy molding compound designed for TO packages. This low stress, low moisture absorption product is a commercial success with many uses on TO applications.

Hysol GR600 SL2 is a green, heat curable epoxy molding compound that can be used in semiconductor packages such as TO252. Furthermore, it meets UL 94 V-0 flammability at 1/8 inch thickness.

Product Family

GR600-SL2/14M4.4G10K

Pelletized - 14MM X 4.4GR | 10kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 10 kg
Gross weight 10.51 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
87 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.03
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
14400000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.30 %
Physical Properties
Spiral Flow @ 175°C
83 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
165 °C
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
5 - 15 s