Hysol GR2822 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Hysol GR2822 | Black Epoxy Mold Compound Hysol GR2822 | Black Epoxy Mold Compound

Main features

  • For Conductive Polymer Tantalum Solid Capacitors
  • Ultra-low stress epoxy mold compound
  • MSL3 260°C - Thin Wall Crack Resistance

Product Description

Hysol GR2822 is a silica filled (88%), black, epoxy molding compound. Despite what the name implies, it is not a newer version of 2820 but an improved version of our gold GR2811. Hysol GR2811 showed poor moisture resistance (crack after MSL3) and discolouration issues under harsh circumstances. GR 2822 was developed to solve those issues and while black, be used for demanding applications.

Hysol GR2822 heat curable EMC, meets JEDEC MSL 3 requirements and is a green product designed for tandalum conductive polymer capacitors. It exhibits very low stress, low moisture absorption and good electrical performance.

Product Family

GR2822/14M3.4G1K

Pelletized - 14MM x 3.4GR | 1kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 1 kg
Gross weight 1.5 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
88 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.98
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
105 °C
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
14000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.26 %
Physical Properties
Spiral Flow @ 175°C
99 cm
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
5 - 20 s

Additional Information

{tab=Applications}

Short Description of {product_name}

Typical applications and uses of {product_name} include:

  • Condutive Polymer Tantalum Solid Capacitors (POSCAP)
  • Other Tantalum Capacitors

Technical Datasheets for {product_name}

TDS (English) Kapton_Technical_Data_Sheet Click to access {product_name} Technical Data Sheet
*Note that only registered users may access technical datasheets

{tab=Packaging Details}

Packaging Details for {product_name}

The following information is specifically related to each unit of measure of {product_name}. If you which to compare this to other product sizes, click on the respective product from the list above and check here for values specific to that product. These values are taken from our internal database and are used in the calculation of the gross weight and packaging dimensions of the goods during shipping. You can use these values to approximate delivery charges using your own carrier.

{/tabs}

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers