Hysol GR2720 | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR2720 Black Epoxy Mold Compound Hysol GR2720 | Black Epoxy Mold Compound

Main features

  • For conductive polymer and AO capacitors
  • Excellent thin wall crack resistance
  • Fast cure for automold equipment

Product Description

Hysol GR2720 is a low stress, black semiconductor-grade epoxy molding compound designed for the encapsulation and protection of Conductive Polymer Capacitors and Aluminum Organic (AO) capacitors.  Polymer conductive capacitors and Aluminum Organic capacitors offer very high capacitance in a very small size. Epoxy molding compounds designed for these packages must have very low stress and very good thin wall crack resistance. This is the only way to be able to pass the MSL performance on these package types. GR2720 excels in both fields and has both low stress and excellent thin wall crack resistance.

Hysol GR2720 is a laser markable, environmentally free, halogen free "green" product, meaning that it doesn't contain any halogens including bromine, antimony or phosphorus flame retardants.  This material is designed to achieve JEDEC Level 1 requirements at 260°C reflow temperature on Aluminum Organic (AO) capacitors as well as conductive polymer capacitors. Its fast cure time also ensures that it is compatible with the latest automold manufacturing equipment. Hysol GR2720 meets UL 94 V-0 Flammability at 1/4 inch (6.35mm) thickness.

Product Family

GR2720/14.3M5G15K

Pelletized - 14.3MM x 5GR | 15kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 15.51 kg
Dimensions 25.5 x 28.5 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Black
Filler Content
79 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.87
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
320000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorption
0.30 %
Physical Properties
Spiral Flow @ 175°C
96.5 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
160 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.7 W/m.K
UL 94 Rating
Flammability rating classification. It determines how fast a material burns or extinguishes once it is ignited. HB: slow burning on a horizontal specimen; burning rate less than 76 mm/min for thickness less than 3 mm or burning stops before 100 mm V-2: burning stops within 30 seconds on a vertical specimen; drips of flaming particles are allowed. V-1: burning stops within 30 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. V-0: burning stops within 10 seconds on a vertical specimen; drips of particles allowed as long as they are not inflamed. 5VB: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may develop a hole. 5VA: burning stops within 60 seconds on a vertical specimen; no drips allowed; plaque specimens may not develop a hole
V0
Mechanical Properties
Molded Shrinkage
0.23 %
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
6 - 15 s

Leading Brands Trust in Our Products and Services