Hysol GR17 | White Epoxy Mold Compound

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

Hysol GR17 | White Epoxy Mold Compound

Main features

  • Reflective compound
  • For Optocouplers
  • High moldability

Product Description

Hysol GR17 is a white, reflective epoxy molding compound used for optical applications. This silica filled (68%) product has been designed to improve light reflectance and workability for optocouplers also knows as photo-couplers, optical isolators, or opto-isolators.

Hysol GR17 cures with heat and can be used for transfer processes. It has been formulated to provide high moldability, low stress and high adhesion to a variety of substrates. Transmissivity is 18.5.

Product Family

GR17/13M4.1G15K

Pelletized - 13MM X 4.1GR | 15kg NET box
1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Box
Net weight 15 kg
Gross weight 16.5 kg
Dimensions 25 x 28 x 26.5 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
White
Filler Content
68 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.75
Chemical Properties
Moisture absorption
0.46 %
Physical Properties
Spiral Flow @ 175°C
50 cm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
182 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.65 W/m.K
Curing Conditions
Transfer Pressure
40 - 85 kg/cm2
Transfer Time
10 - 15 s

Additional Information

Storage

Store product in the unopened container in a dry location. Storage information may be indicated on the product container labeling.

Optimal Storage: 5°C or below, in closed containers. After removal from cold storage, the material MUST be allowed to come to room temperature, in the sealed container, to avoid moisture contamination. The suggested waiting time for a standard 15 kg carton box is 24 hours.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers