LOCTITE ECCOBOND UV8800M

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND UV8800M

Main features

  • UV Cure
  • Cures rapidly
  • Excellent adhesion

Product Description

LOCTITE UV8800M epoxy encapsulant is developed to meet high temperature thermal cycling specifications. It UV cures to form a hard translucent coating when exposed to UV light of sufficient intensity. The curing of the product is not inhibited by oxygen, resulting in excellent surface cure.

LOCTITE UV8800M exhibits viscosity characteristics and dearated condition that make it suitable for accurate dispensing with excellent shape control. This encapsulant is typically used for CSP and BGA packages and is, among others, used on Glass, Epoxy, Polyimide and Polyester substrates.

UV Cure Condition

Medium pressure mercury lamp:

  • Light Dose, mW/cm² 100
  • Exposure Time, seconds 2
  • UV radiation, , nm (UVA) 315 to 400
Product Family

UV8800M/1V0

1Kg Bottle - 1228111

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.6
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
29 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
3,000 mPa.s

Additional Information

LOCTITE UV8800M can be cured by irradiation with ultraviolet and visible light as well as LED-UV light with single wavelength distribution of sufficient intensity. Cure rate and depth of cure depend on the intensity, spectral distribution of the light source, exposure time and light transmittance of the substrate through which the light must pass.

alt

Leading Brands Trust in Our Products and Services