LOCTITE ECCOBOND LUX OGRFI146T

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND LUX OGRFI146T

Main features

  • Low refractive index
  • Photocurable
  • Cures in shadowed areas

Product Description

LOCTITE ECCOBOND LUX OGRFI146T photocurable adhesive is formulated to enhance productivity in the assembly of optical, fiber optic, and optoelectronic devices. It is an optical grade, clear acrylate with a low refractive index.

LOCTITE ECCOBOND LUX OGRFI146T contains a secondary thermal cure mechanism for applications that contain shadowed areas where light is unable to penetrate. The secondary thermal cure can be done in a conventional box or convection conveyor ovens.

UV Cure

  • 500 mW/cm² for 8 seconds
Product Family

OGRFI146T/3A0

3cc Syringe - 1200688
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 18 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Unit of measure Syringe
Net weight 3.6 g
Gross weight 9.39 g
Dimensions 2.8 x 1.4 x 7.6 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Refractive index
The refractive index determines how much the path of light is bent, or refracted, when entering a material. It is calculated by taking into account the velocity of light in vacuum compared to the velocity of light in the material. The refractive index calculation can be affected by the wavelength of light and the temperature of the material. Even though it is usually reported on standard wavelengths it is advised to check the TDS for the precise test parameters.
1.45
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
2184 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
188 °C
Chemical Properties
Water Absorption
1.5 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1,250 mPa.s