LOCTITE ECCOBOND LUX OGR150THTG

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND LUX OGR150THTG

Main features

  • Non conductive
  • Photocurable
  • Cures in shadowed areas

Product Description

LOCTITE ECCOBOND LUX OGR150THTG photocurable, acrylate adhesive is designed for high throughput optoelectronic assembly operations. It is a low viscosity, transparent, dual cure acrylate (UV and heat) for cavity fill of test ICs.

LOCTITE ECCOBOND LUX OGR150THTG contains a secondary thermal cure mechanism for applications that contain shadowed areas where light is unable to penetrate. The secondary thermal cure can be done in conventional box or convection conveyor ovens.

UV Cure

  • UV 365 nm with 110 mW/cm²at the bondline

Secondary Thermal Cure

  • 1 hour @ 100°C or
  • 2 hours @ 85°C
Product Family

LUXOGR150THTG/3A0

3cc Syringe - 1200996
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 18 days
CA Shipping in 12 weeks
EU Shipping in 40 days
Packaging
Unit of measure Syringe
Net weight 3.6 g
Gross weight 10 g
Dimensions 2.8 x 1.4 x 7.6 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
2184 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
145 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1,000 mPa.s

Additional Information

LUX OGR150THTG Transmission vs Wavelength

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers