LOCTITE ECCOBOND FP4654

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND FP4654

Main features

  • High purity
  • Self levelling
  • Low stress

Product Description

LOCTITE® ECCOBOND FP4654 is a low stress, Fill Encapsulant designed for larger cavity-fill or dam-and-fill applications. It is self levelling, jettable and provides an excellent thermal stability.

LOCTITE® ECCOBOND FP4654 has one of the lowest CTE α1 among the series (13ppm) and is our closest "mold compound" simulator with the highest (80%) Silica filler loading.

Recommended Cure Schedule

  • 30 minutes @ 125°C plus
  • 90 minutes @ 165°C
Product Family

FP4654/55E0

55 CC Syringe - 1634265

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
72 hours
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.85
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
146 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
32,000 mPa.s

Leading Brands Trust in Our Products and Services