LOCTITE ECCOBOND EO7029

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Loctite Eccobond EO7029

Main features

  • Smartcard applications
  • Non conductive
  • Die attach & Encapsulant

Product Description

LOCTITE® ECCOBOND EO 7029 is a highly thixotropic, one component epoxy encapsulant with fast curing capability at moderate temperature and is designed specifically as non conductive die attach for smart card application and adjusted to be thixotropic to avoid flowing during cure. It's a great and cost effective 2 in 1 solution, similar to EO 7021.

 

Cure Schedule

  • 5min @ 150°C.  - Robust non-stress sensitive components
  • 1hour @ 120°C.  - Stress sensitive components 
Product Family

EO7029/30D0

30cc Syringe - 464876
1. Select Package Type
2. Select Package Size

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 30 days
Packaging
Unit of measure Syringe
Net weight 37 g
Gross weight 52 g
Dimensions 4 x 4 x 12.4 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.20
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
110 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
48,000 mPa.s