LOCTITE ECCOBOND 7010C DAM

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND 7010C DAM

Main features

  • Dam
  • Low CTE
  • High purity

Product Description

LOCTITE ECCOBOND DAM 7010C is a black epoxy semiconductor encapsulant, formulated to be used in combination with a "fill" encapsulant LOCTITE ECCOBOND FIL 7010C as a dam encapsulant. It is specially designed for glob top, chip on board applications where protection of wire bonded bare IC is required. This two material combination is also suited for the protection of multiple chips and for encapsulating components where a well-defined glob height and flat surface are required.

LOCTITE ECCOBOND DAM 7010C has good crack, chemical and thermal resistance along with low thermal expansion. This SVHC free, REACH compliant, high purity, low sag material operates at -40 to 150ºC and is typically used for glob top applications and the encapsulation of bare wire bonded semiconductors.

Cure Schedule

  • 2 hours @ 140°C
  • 1 hour @ 100°C plus 1 hour @ 150°C (Low Stress)

Recommended Dispensing Settings

  • For best results, dispense onto substrate warmed to 80°C, and then optimize by reducing the needle size, dispensing pressure, and speed to achieve the desired dam width and height.
Product Family

DAM7010C/30D0

30cc Syringe - 2648755
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 38 days
CA Shipping in 12 weeks
EU Shipping in 25 days
Packaging
Unit of measure Syringe
Net weight 40 g
Gross weight 61 g
Dimensions 4 x 3.1 x 11.8 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black
Density (g)
1.90 g/cm3
Filler Content
81 %
Filler Size Cut
20 - 120 µm
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
135 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.78 W/m.K
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
22 kV/mm
Surface Resistivity
e.9e 15 Ohms/sq
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.00000000000000896 Ohms⋅cm
Chemical Properties
Water Absorption
0.10 %
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
3.3
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
80,000 - 105,000 mPa.s
Young's modulus
11,000 MPa

Additional Information

For additional information, consult the data package in the documents section.

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers