LOCTITE ECCOBOND D125 F DR

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND D125 F DR

Main features

  • Low water absorption
  • Low exotherm
  • Non-sag

Product Description

LOCTITE D 125 F DR is a epoxy surface-mount adhesive designed for high-speed dispensing.

LOCTITE D 125 F DR is used in a wide array of applications, including chip capacitors, chip resistors, SOTs, SOICs, and PLCCs. 

 

Product Family

D125FDR/310K0

310ml cartridge - 1189477

Loading pricing…

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.275
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
85 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
0.3 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
1000000000000000 Ohms⋅cm

Additional Information

TYPICAL CURING PERFORMANCE 

IR or Convection Conveyor Oven
20 minutes @ 100°C
7 minutes @ 110°C
2.5 minutes @ 120°C
1.5 minutes @ 150°C

Convection Box Oven

30 minutes @ 100°C
20 minutes @ 110°C
10 minutes @ 120°C 
5 minutes @ 150°C