LOCTITE ECCOBOND 931-1T1N1

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

Loctite Eccobond 931-1T1N1

Main features

  • Low viscosity
  • Low temperature cure
  • Extraordinary adhesion

Product Description

LOCTITE® ECCOBOND 931-1T1N1 die attach adhesive is designed for smart card applications. This clear, low viscosity epoxy develops extraordinary adhesion on substrates such as glass, Alumina, Ferrite, Aluminum and steel after a low temperature cure. It has low ionics and is fairly stable when exposed to printing inks. 

LOCTITE® ECCOBOND 931-1T1N1 is used as a die attach for smartcards to bond the wire bonded module onto the plastic card using low temperature cure. It's also being used in multiple bond lines, in assembling inkjet and thermal printer heads, for die attach and for assembling several other components (metal, ceramic and some plastics) around the print head.

LOCTITE® ECCOBOND 931-1T1N1 is fairly transparent at least in thin layers, although there is no spec or control over the optical properties. It is an epoxy, so becomes more yellow on aging at high temperature. It is very reactive, with short work life & critical storage conditions. It is corrosive and a strong skin sensitizer, so should be kept away from skin & eyes. And in pre-mixed form it is strongly exothermic. The SADT temperature is low, so it cannot be transported by air, and there are severe restrictions on shipping by road & sea. Having said that, it fully makes up for those with its end properties and for special applications it can make a difference.

Recommended Cure Schedule

  • 2 hours @ 100°C
  • 2 hours @ 60°C
Product Family

931-1T1N1/30D0

30cc Syringe - 1456632
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 25 days
Packaging
Unit of measure Syringe
Net weight 35.1 g
Gross weight 53 g
Dimensions 4 x 3.1 x 12 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
2 hours
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
4 hours
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
2.8
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
2,400 mPa.s

Additional Information

Storage and Handling of Die Attach Epoxies

Proper storage and handling are crucial aspects of working with one part frozen epoxies. From the moment your shipment of LOCTITE ABLESTIK or LOCTITE ECCOBOND arrives, to the careful thawing process before use, each step ensures these high-performance adhesives live up to their reputation. Whether you’re bonding dies, encapsulating packages or assembling automotive components, following these guidelines will help you achieve flawless dispensing and curing performance and achieve the stated specifications. Read more on our blog on a practical guide in handling and storing die attach pastes.

 

 Read the Blog

Blog Banner

Further Reading on Die Attach Materials

Bare copper

Bare Copper Substrate Die Bonding

Rose Anne Acedera, August 2025
Blog 2 Banner

Optimizing Die Attach Dispensing

George Kountardas, May 2025