Main features

  • Adhesion promoter
  • Flexible aliphatic backbone
  • Long Alkyl chain

Product Description

MM-281 is a long chain maleimide terminated carboxylic acid. It is a useful intermediate for the synthesis of ester and amide linked thermoset monomers. The long alkyl chain provides flexibility and hydrophobicity

ΜΜ-281 has a flexible aliphatic backbone and maleimide and carboxylic acid functional groups that aid in adhesion promotion in free-radical or in epoxy/(meth)Acrylate hybrid adhesives . It is recommended for use as an intermediate for maleimide functional resins and the main difference with the seemingly identical MM-211 is the twice as long alkyl chain. 

Product Family

MM281/100GJ0

100gr Jar
1. Select Package Type

Loading pricing…

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Unit of measure Jar
Net weight 0.05 kg
Gross weight 0.24 kg
Dimensions 6 x 6 x 13 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White powder
Molecular weight
281 g/mol
Thermal Properties
Decomposition Temperature
250 °C