MM211 | Maleimide adhesion promoter Additive

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

MM211 | Maleimide adhesion promoter Additive

Main features

  • Adhesion promoter
  • Flexible aliphatic backbone
  • Maleimide and carboxylic groups

Product Description

MM-211 is an intermediate chain length, maleimide, terminated carboxylic acid. It is a useful intermediate for the synthesis of ester and amide linked thermoset monomers. The alkyl chain provides flexibility and hydrophobicity.

MM-211 is recommended for use as a synthetic intermediate for maleimide functional resins. It may also be used as an adhesion promoter in free-radical or epoxy/(meth)acrylate hybrid adhesives to bind on metal surfaces.

 

Product Family

MM211/J60K

50gr Sample Jar
1. Select Package Type

Loading pricing…

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Unit of measure Jar
Net weight 0.05 kg
Gross weight 0.24 kg
Dimensions 6 x 6 x 13 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
White powder