MM-204 High Tg Mono-Functional Acrylate Monomer

Harmonization Code : 2916.12 | Unsaturated acyclic monocarboxylic acids and their anhydrides, halides, peroxides, peroxyacids, and their derivatives

MM-204 Dicyclopentadiene Acrylate High Tg Mono-Functional Acrylate Monomer MM-204 High Tg Mono-Functional Acrylate Monomer

Main features

  • Hydrolytically resistant
  • Low Viscosity
  • High Glass Transition Temperature (Tg)

Product Description

MM-204 dicyclopentadiene acrylate is a mono-functional acrylate monomer. It has low shrinkage and a high glass transition temperature upon cure. The secondary ester linkage is resistant to hydrolysis.

MM-204 is recommended for use as a reactive diluent for UV or peroxide cured resins, coatings or adhesives. It can also be used to improve stereolithographic processes for high-temperature applications.

Highlights

  • Low viscosity
  • Hydrolytically resistant
  • High glass transition temperature
  • Diluent for thermoset resins
  • Low cure shrinkage
  • High Tg

Typical Physical and Chemical Properties

PROPERTY METHOD RESULT

  • Appearance at Room Temperature: Light tan liquid
  • Viscosity @ 25°C (typical): 50 cPs using Haake Rheometer
  • Functionality:1
  • Molecular Weight: 204 daltons
  • Recommended Storage: At 5°C or below
Product Family

MM-204/J60B

1kg jar
1. Select Package Type

Loading pricing…

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.1 kg
Dimensions 10 x 10 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Light Tan Liquid
Functionality
1
Molecular weight
204 g/mol
Other Properties
Storage Temperature
5 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
50 mPa.s