CS-697 | Polyglycidyl Ether Cyclosiloxane
Harmonization Code : |
Main features
- Low viscosity
- Compatible with organic resins
- For formulating adhesives
Product Description
CS-697 is a polyglycidyl ether cyclosiloxane monomer. The structure above shows a representation of the predominant component. Low viscosity and low color make it ideal for formulating adhesives. This resin is very compatible with most organic resins.
CS-697 is a colorless multifunctional monomer with low epoxy equivalent weight and low chloride that is thermally stable and non yellowing when exposed to UV.
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.3 kg
Dimensions 10 x 10 x 20 cm
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Appearance
Colorless liquid
Appearance at room temperature.
Molecular weight
697 g/mol
Physical Properties
Viscosity
200 mPa.s
Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application