BMI-2500 | Imide extended Bismaleimide powder

Harmonization Code : 2925.19.95.90 | Carboxyimide-function compounds (including saccharin and its salts) and imine-function compounds : Imides and their derivatives; salts thereof : Other : Other : Other

Main features

  • Hydrophobic
  • Toughener
  • Increased modulus and Tg

Product Description

BMI-2500 has been designed to extend the range of applications suitable for use with the Designer Molecules, Inc. imide extended bismaleimide oligomers to those in need of higher Tg and modulus. The material has excellent low pH hydrolytic resistance and thermal stability. As an additive it can improve rheological properties by increasing the thixotropic properties of a liquid monomer composition. This feature in turn can help to reduce resin bleed out on a variety of surfaces. It is soluble in most aromatic and aliphatic solvents such as toluene, xylene, NMP, etc. It can be processed in a resin system as a solid or dissolved in a solvent.

BMI-2500 is recommended for use as an additive to increase flexibility, hydrophobicity and thixotropy. When used as a base resin, it can produce films that are tough, flexible and demonstrate good peel strength. BMI-2500 is compatible with PPE and Acrylates for free radical reaction and epoxy with anionic cure.

Product Family

BMI-2500/1J0

1Kg Jar
1. Select Package Type

Loading pricing…

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Unit of measure Jar
Net weight 1 kg
Gross weight 1.2 kg
Dimensions 8 x 8 x 15 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Light Yellow
Functionality
2
Thermal Properties
Decomposition Temperature
438 °C
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
140 °C
Weight Loss @ 300°C
0.5 %
Other Properties
Storage Temperature
Room temperature °C
Chemical Properties
Water Absorption
0.25 %