COOLINQ SG-25 | Graphite heat spreader

Harmonization Code : 6815.11.00.00 | Articles of stone or of other mineral substances, not elsewhere specified or included; Non-electrical articles of graphite or other carbon; Carbon fibres and articles of carbon fibres

COOLINQ SG-25 Graphite heat spreaders

Main features

  • 25um Graphite
  • Light weight and flexible
  • Excellent thermal conductivity

Product Description

COOLINQ SG-25, is your ideal solution for achieving superior thermal management in various industries, from consumer electronics to aerospace and more. This innovative graphite sheet is engineered to efficiently distribute and dissipate heat, ensuring consistent peak performance of electronic components, even under the most demanding conditions.

COOLINQ SG-25 stands out with its ultra-thin profile, measuring just 0.025mm in thickness. This exceptional thinness, combined with its lightweight and flexible nature, allows for seamless integration into electronic devices without adding unnecessary bulk. Its versatility extends beyond consumer electronics, making it a preferred choice for applications in the automotive, aerospace, and industrial sectors.

One of the standout features of COOLINQ SG25 is its exceptional durability. It is engineered to withstand wear and tear, providing long-lasting thermal management solutions. Moreover, its ease of integration sets it apart from the competition. Unlike rigid metal heat spreaders, COOLINQ SG25 can be easily cut, shaped, or layered to precisely fit your unique application. You can effortlessly cut, shape, or layer it to match your specific requirements, making it a versatile addition to your thermal management toolkit.

Key Applications:

  • Consumer Electronics: COOLINQ SG25 enhances the thermal performance of everyday gadgets, ensuring they operate optimally, even under challenging conditions.
  • Automotive: Elevate the efficiency and reliability of automotive electronics, maintaining their performance across diverse operating conditions.
  • Aerospace: In critical aerospace applications, COOLINQ SG25 stabilizes electronic systems and extends their operational lifespan.
  • Industrial Equipment: Improve the performance and longevity of industrial electronics and machinery.
Product Family

CL-SG25/14.7X7

14.7cm x 7cm Sheet

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)
2.1 g/cm3
Total Thickness
Total thickness is taking into account all the films, coatings, adhesives, release liners and special layers and is the maximum thickness of a film or tape.
0.025 μm
Thermal Properties
Operating Temperature
-40 - 400 °C
Specific Heat Capacity
Specific heat capacity is the amount of heat energy required to raise the temperature of a substance per unit of mass. The specific heat capacity of a material is a physical property. It is also an example of an extensive property since its value is proportional to the size of the system being examined.
0.94 J/(g⋅°C)
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
1500 W/m.K

Additional Information

Frequently Asked questions

How are Graphite sheets made?

COOLINQ SG25 Graphite Sheets are manufactured using advanced processes that ensure consistency and precision. Our proprietary manufacturing techniques result in sheets with uniform thickness, exceptional thermal conductivity, and minimal defects. This level of quality control ensures that every sheet you receive meets the highest industry standards.

Are graphite sheets better than metal spreaders?

COOLINQ SG25 Graphite Sheets have a clear advantage over traditional heat-spreading technologies, particularly those of the same thickness. Conventional materials like metal heat spreaders are heavier and less flexible, limiting their applicability in compact and lightweight electronic devices. In contrast, COOLINQ SG25's ultra-thin profile at just 0.025mm offers an unprecedented combination of heat spreading efficiency and flexibility. It's remarkably lightweight and can be effortlessly integrated into even the most space-constrained electronics.

What is the Thermal Conductivity of Graphite sheets?

What sets COOLINQ SG25 apart is its remarkable thermal conductivity, which surpasses that of many other materials at the same thickness. Thanks to its highly oriented pyrolytic graphite (HOPG) composition, it excels at rapidly conducting heat in both the X-Y (1500 W/mK) and Z (10W/mK) directions. This makes it an ideal choice for scenarios where efficient heat dissipation is paramount.

 

Handling and Storage

  • Handling: To prevent contact with graphite powder, it is advisable to wear gloves and a smock during handling.

  • Storage: Store the product away from potential ignition sources and oxidizing materials. Ensure it is kept in a cool, dry place, sealed tightly within a container.

Operator Protection

  • Adequate ventilation is recommended during operation.

  • While no specific skin protection is necessary, it is advisable to use eye protection when working with the product.

  • Due to its high thermal conductivity, avoid direct contact with the product when the operating temperature exceeds 60°C or falls below freezing.

Safety Precautions

  • Strictly adhere to the specified working temperature range of -50 to 250°C.

  • Avoid using the product with acidic substances.

  • Prevent any rough handling, rubbing, or collision with sharp objects.