OP-272 | Nano-Scale Adhesion-Promoting Surface Treatment

Main features

  • Improved adhesion strength of paints/coatings on metal surfaces
  • No outgassing
  • No stress build-up on the substrates

Product Description

Aculon OP-272 is a nano-scale, isopropanol-based surface treatment engineered to significantly enhance adhesion to metal substrates for coatings that cross-link via hydroxyl functional groups, including urethane, melamine-formaldehyde, and phenolic-epoxy systems. Designed for use in demanding electronics, industrial, and coating applications, OP-272 delivers a thin (2–4 nm), invisible, and stable monolayer that strengthens interfacial bonding without altering substrate appearance or introducing mechanical stress.

It integrates easily into existing production lines using conventional wet application methods such as dipping, spraying, or wiping, and provides exceptional chemical resistance and coating compatibility.

Applications:

  • Enhance epoxy adhesion on metal lead-frames in electronics
  • Improve bonding of urethane and phenolic-based over-mold compounds
  • Prevent delamination in finished coatings or laminates
  • Boost adhesion of melamine-formaldehyde coatings for heat- and chemical-resistant applications
Product Family

OP-272/240ML

240ml bottle
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 8 weeks
CA Shipping in 8 weeks
EU Shipping in 8 weeks
Packaging
Unit of measure Bottle
Net weight 0.4 kg
Gross weight 0.6 kg
Dimensions 10 x 13 x 13 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
clear
Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
82 °C
Electrical Properties
Visible Light Transmission
100 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
2 mPa.s

Additional Information

Surface Preparation/ Cleaning:
Ensure that the surface is free of any grease, fingerprints or dirt (i.e., water break free). This can be accomplished by first degreasing the surface with solvents or by rinsing with soap and water. The next step is to remove monolayer-scale contaminants. This is typically performed by using a cleaner specifically designed for the metal you are working with. Contact Aculon if you are unsure what cleaner to use and we will recommend one best suited for your application. The substrate should be water break - free before continuing to coating steps.

Treatment Application:
Spray: Spray the solution onto the substrate using doubl e passes. Post-application curing is recommended for best performance. Spray Equipment Suggestions: HVLP (Binks Mach 1), HVLP
(Devilbiss JGHV), Air Atomizatation (Devilbiss MBC gun), and Airless (Graco Model 225-292 President Pump Series A)

Dip: – Immerse the substrate in the solution for five minutes. If a shorter dip time is necessary, then a post-cure is recommended for optimal performance (sonication while dipping can boost performance in some cases).

Dip Coating with Sonication: Ensure the substrate is clean. Completely submerge the substrate in the solution and sonicate for five minutes. Remove substrate from the solution and allow to air dry , preferably in a clean area.

Drying/ Curing: If curing is necessary (short dip times or spray-application), the treated substrates are best cured at 120C peak metal temperature for approximately 30 seconds. For silicon and titanium
oxides, lengthening the cure time to 5 minutes is recommended.
*Note: If OP-272 is being used to adhere a high viscosity or low-reactive resin system, especially if such coating is not cured after application, then it is suggested to do a post cure rinsing step (or post-treatment rinse if curing was
not performed) for best performance. In certain cases it is also possible to directly blend the active materials into a coating; contact an Aculon representative if this approach is of interest to you.

Safety, Handling, Storage, Shelf Life:
Store in a cool (~25C) and dry area, and keep away from direct sun light. See this product’s MSDS for proper handling and fire hazard data. When stored properly, product has a 2 year shelf life from the date it is opened.