LOCTITE ABLESTIK QMI 516

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK QMI 516

Main features

  • Electrically conductive
  • Hydrophobic
  • Snap cure

Product Description

LOCTITE ABLESTIK QMI516 is a silver filled conductive adhesive for attachment of integrated circuits and components to metal leadframes advanced substrates, including: SBGA’s, PBGA’s, array packages, tape packs and CSP’s. This material is hydrophobic and stable at high temperatures. These features produce void-free bonds lines with excellent interfacial adhesion strength to a wide variety of organic and metal surfaces, including solder mask, BT, FR, polyimide, Au, Kapton™ and Mylar™.

A package or device manufactured with LOCTITE ABLESTIK QMI516 will have good resistance to delamination and “popcorning” after exposure to reflow temperatures. The adhesive also has excellent electrical and thermal conductivity properties. LOCTITE ABLESTIK QMI516 can be cured in a conventional oven, on a snap cure oven, or utilize SkipCure™ processing on a die bonder or wire bonder. The material is formulated to produce cure onset below 100°C. This can reduce or eliminate the need to pre-dry organic substrates prior to the die attach process.

LOCTITE ABLESTIK QMI516 is a long standing product with no plans to be discontinued. Nevertheless, the risk of running into raw material disruptions and minimum batch size challenges with QMI 516 over time is higher than with other high-volume runners. That’s why, for new applications, we recommend qualifying LOCTITE ABLESTIK 2100A with similar properties and applications.

Snap Cure 

  • 10 seconds @ 150°C

Oven Cure

  • 15 minutes @ 150°C
Product Family

QMI516/5B0

5cc Syringe - 447235
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Unit of measure Syringe
Net weight 0.0197 kg
Gross weight 0.0397 kg
Dimensions 5 x 5 x 7 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
24 hours
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
3.93
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
33 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
4.2 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.0017 Ohms⋅cm
Chemical Properties
Moisture absorption
0.2 %
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
3
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
8,000 mPa.s

Additional Information

How do Bismaleimide based materials fair against bleeding?

Bleeding is a known “side effect” of QMI products based on BisMaleImide (BMI) resin. The relatively low BMI resin viscosity allows higher filler loading and this makes this resin popular for semiconductor die attach use (next to its higher temperature and moisture resistance vs epoxies for instance). By using very fast “snap cure” profiles like most semiconductor companies do, bleeding can be controlled. Acrylate resin based products like CA 3556HF show less bleeding in general.

Bleeding can be also controlled by surface treatments, curing process and adding anti-bleed agents to the adhesives.

Sometimes if you take the relatively short pot life at 25C and high reactivity of QMI resins into account, next to its higher bleeding and higher resin cost base, we could suggest to focus on CA 3556HF and lower silver content ICP 8282 for specific applications. It is all application dependent and we are happy to help you choose.