LOCTITE ABLESTIK EMI 8890SB

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK EMI 8890SB

Main features

  • Conformal EMI shielding
  • Excellent adhesion on EMC
  • Spray coating

Product Description

LOCTITE ABLESTIK EMI 8890SB is an electrically conductive adhesive designed to achieve robust electromagnetic interference (EMI) shielding performance with extremely thin coating thickness at a single micrometer level for package level shielding applications.

LOCTITE ABLESTIK EMI 8890SB has robust adhesion to mold compound, epoxy, copper, gold and silver surfaces. When spray-coated, this material can be atomized to highly fine droplets for excellent uniformity at low to high coating thicknesses which can be controlled by equipment parameters.


Cure Schedule

  • 60 minutes @ 175°C
Product Family

EMI8890SB/30C0

20cc in 30cc Syringe - 2741349
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 23 days
CA Shipping in 12 weeks
EU Shipping in 16 weeks
Packaging
Unit of measure Syringe
Net weight 50 g
Gross weight 68 g
Dimensions 3 x 3 x 11.8 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.000007 Ohms⋅cm
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
500 mPa.s

Additional Information

 

Thawing graph of EMI8890SB

Directions for Use

1. Thawed material should immediately be placed on dispense equipment for use.

2. If the adhesive is transferred to a final dispensing reservoir, care must be exercised to avoid entrapment of contaminations and/or air into the adhesive.

3. Adhesive must be completely used within the product's recommended work life.

4. No special surface treatment is needed for the substrate surface before applying this material.

5. Prior to material application, it is recommended that the substrate be handled with care to prevent any organic contamination and/or residue.

Storage

Store the product in the unopened container in a dry location. Storage information may be indicated on the product container labeling.

 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers