LOCTITE ABLESTIK EMI 8660S

Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

LOCTITE ABLESTIK EMI 8660S

Main features

  • Conformal EMI shielding
  • Excellent adhesion on EMC, Au, Ag
  • Spray, Print, Dispense

Product Description

LOCTITE ABLESTIK EMI 8660S is an electrically conductive adhesive designed to achieve robust electromagnetic interference (EMI) shielding performance with extremely thin coating thickness at a single micrometer level for package level shielding applications.
The material has robust adhesion to mold compound, epoxy, copper, gold and silver surfaces. When spray-coated, this material can be atomized to highly fine droplets for excellent uniformity at low to high coating thicknesses which can be controlled by equipment parameters.

LOCTITE ABLESTIK EMI 8660S is a sprayable, printable or dispensable silver sintering coating that exhibits high thermal and electrical conductivity. With good workability and a long work life, this material is typically used for RF, Wireless components, memories, sensors and other sensitive device applications.

Cure Schedule

  • 60 minutes @ 175°C
Product Family

EMI8660S/20D0

20cc in 30cc Syringe - 2343744
1. Select Package Type

Loading pricing…

Packaging
Unit of measure Syringe
Net weight 0.082 kg
Gross weight 0.142 kg
Dimensions 8 x 8 x 10 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
24 hours
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.00001 Ohms⋅cm
Physical Properties
Thixotropic index
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten. A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads. It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
3
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
340 mPa.s