LOCTITE ABLESTIK ECF 564AHF

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

LOCTITE ABLESTIK ECF 564AHF

Main features

  • High flow version of 564A
  • Excellent thermal conductivity
  • Passes Mil 5011 and NASA outgassing

Product Description

LOCTITE ABLESTIK ECF 564AHF adhesive film is designed for use in hybrid packages where outgassing and ionic contamination must be kept to a minimum. This isotropically electrically conductive adhesive film has excellent thermal conductivity and comes with a glass fabric carrier.

LOCTITE ABLESTIK ECF 564AHF is the High flow version of ECF 564A and meets the NASA outgassing requirements and those of MIL-STD883C, Method 5011

 

Cure Schedule

  • 2 hours @ 150°C
Product Family

ECF564AHF/6X6T6

6 x 6 inch - 6mil sheet - 1202968
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 26 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Unit of measure Sheet
Net weight 6.225 g
Gross weight 6.325 g
Dimensions 15.2 x 15.2 x 0 cm
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
122 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3 W/m.K
Weight Loss @ 300°C
0.15 %
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.0004 Ohms⋅cm