LOCTITE ABLESTIK DX20C

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK DX20C

Main features

  • Translucent
  • Non conductive
  • For GaN LEDs

Product Description

LOCTITE ABLESTIK DX20C dielectric adhesive offers excellent adhesion strength, especially at wire bonding process temperature to minimize defect rate at assembly. It features strong heat / UV resistance and can be applied by pin transfer, stamping and dispensing.

LOCTITE ABLESTIK DX20C is a translucent, one component die attach that doesn't yellow and has excellent adhesion for LED applications on GaN (Gallium Nitride) substrates.

 

Cure Schedule

  • 1 hour @ 170°C
Product Family

DX20C/30D0

30CC Mushashi - 1363063

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.17
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
120 hours
Chemical Properties
Moisture absorption
0.6 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
12,000 mPa.s