LOCTITE ABLESTIK CE8500

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK CE8500

Main features

  • Flexible
  • Low stress
  • Bond mismatched substrates

Product Description

LOCTITE® ABLESTIK CE 8500 is a solventless epoxy adhesive that combines low stress with good adhesion on nearly all surfaces. This silver filled, electrically conductive, modified, epoxy offers low stress and can be used to bond mismatched adherents due to its flexibility.

LOCTITE® ABLESTIK CE 8500 can operate in temperatures ranging from -45°C to 200°C and due to its thermal conductivity is typically used for substrate attach, heat sink attach and sensor attach.

Cure Schedule

  • 90 minutes @ 120°C or
  • 40 minutes @ 150°C or
  • 15 minutes @ 175°C

 

Product Family

CE8500/10C0

10cc Syringe - 1189575
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 34 days
CA Shipping in 12 weeks
EU Shipping in 20 days
Packaging
Unit of measure Syringe
Net weight 25 g
Gross weight 36 g
Dimensions 3 x 2.3 x 9.1 cm
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
24 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
4 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.0002 Ohms⋅cm
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
10 %
Chemical Properties
Moisture absorption
1.5 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
120,000 mPa.s