LOCTITE ABLESTIK CDF 815P

Harmonization Code : 7115.90.00.00 | Other articles of precious metal or of metal clad with precious metal : Other

LOCTITE ABLESTIK CDF 815P

Main features

  • Electrically conductive
  • Thermally conductive
  • QFN, SOIC, SO

Product Description

LOCTITE ABLESTIK CDF 815P highly filled, conductive die attach adhesive is designed to provide high thermal and electrical conductivity in the attachment of integrated circuits and components onto metallic leadframes. This adhesive exhibits strong adhesion to various wafer metallizations and leadframe finishes. It can be used in a variety of die sizes ranging from 0.2mm x 0.2mm to 4mm x 4mm.

LOCTITE ABLESTIK CDF 815P exhibits high MSL reliability and excellent in package thermal and electrical resistance. It is typically used for die attach in QFN, SOIC and SO packages.

Cure Schedule

  • 30 minute ramp from 25°C to 200°C, hold 60 minutes at 200°C
  • 30 minute ramp from 25°C to 175°C, hold 60 minutes at 175°C
Product Family

CDF815P/25N6

25 x 6" circles Roll - 1793244

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
15 µm
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
2160 hours
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
12 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.4 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.0002 Ohms⋅cm

Additional Information

 

 

CDF 800P - Die attach film property comparison