LOCTITE ABLESTIK 84-3LV
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Solvent-free
- Long work life
- One component
Product Description
LOCTITE ABLESTIK 84-3LV adhesive is designed for die attach applications. It is a non conductive, solvent free material that is used as an electrically insulating adhesive.
LOCTITE ABLESTIK 84-3LV is a Low Viscosity version of LOCTITE ABLESTIK 84-3. It can be applied by stamping or syringe dispensing.
Cure Schedule
- 1 hour @ 150°C
- 2 hours @ 125°C
Packaging
Unit of measure Syringe
Net weight 9 g
Gross weight 17 g
Dimensions 3 x 2.3 x 9.2 cm
Technical Specifications
General Properties
Work life @25°C
336 hours
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate.
It is based on the change in viscosity and it can rely on the application requirements.
Thermal Properties
Glass Transition Temperature (Tg)
66 °C
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding.
The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
Thermal Conductivity
0.5 W/m.K
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance.
Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
Weight Loss @ 300°C
0.12 %
Physical Properties
Thixotropic index
1.6
Thixotropic Index is a ratio of a material s viscosity at two different speeds in Ambient temperature, generally different by a factor of ten.
A thixotropic material s viscosity will decrease as agitation or pressure is increased. It indicates the capability of a material to hold its shape. Mayonnaise is a great example of this. It holds its shape very well, but when a shear stress is applied, the material easily spreads.
It helps in choosing a material in accordance to the application, dispense method and viscosity of a material.
Viscosity
12,500 mPa.s
Viscosity is a measurement of a fluid’s resistance to flow.
Viscosity is commonly measured in centiPoise (cP). One cP is defined as
the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP.
A product like honey would have a much higher viscosity -around 10,000 cPs-
compared to water. As a result, honey would flow much slower out of a tipped glass than
water would.
The viscosity of a material can be decreased with an increase in temperature in
order to better suit an application