LOCTITE ABLESTIK 84-1LMIT1

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 84-1LMIT1

Main features

  • Electrically conductive
  • High thermal conductivity
  • Faster Screen printing

Product Description

LOCTITE ABLESTIK 84-1LMIT1 epoxy adhesive is designed for medium sized die attach applications. It is designed for screen printing using 325 mesh. This T1 version has lower viscosity, for finer and faster screen printing compared to 84-1LMIT.

LOCTITE ABLESTIK 84-1LMIT1 meets the military requirements of MIL-STD883C, Method 5011 and also passes NASA outgassing requirements. It is an electrically and thermally conductive, solvent free adhesive with low viscosity and good adhesion.

Cure Schedule

  • 1 hour @ 150°C 
  • 2 hours @ 125°C
Product Family

84-1LMIT1/3A0

3CC Syringe - 1199981
1. Select Package Type

Loading pricing…

Product availability
US Shipping in 28 days
CA Shipping in 12 weeks
EU Shipping in 50 days
Packaging
Unit of measure Syringe
Net weight 12.6 g
Gross weight 17.35 g
Dimensions 3.2 x 1.4 x 7.6 cm
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
103 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
3.6 W/m.K
Weight Loss @ 300°C
0.16 %
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.0005 Ohms⋅cm
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
22,000 mPa.s