3M™ Double Sided Foam Tape 9528
Harmonization Code : 3919101200 | Of poly(vinyl chloride) or of polyethylene in rolls of a width not exceeding 20cm
Main features
- Rubber adhesive delivers quick “grab” for fast bonding
- Adhesive on both sides for easy mounting and joining
- Provides light conformability and consistent thickness
Product Description
3M™ Double Coated Foam Tape 9528 is a 0.8 mm thick, closed-cell polyethylene foam tape coated on both sides with a rubber-based adhesive. Designed for lower-performance applications, it offers high initial tack (“high grab”) for quick bonding of lightweight materials. The foam construction provides basic conformability and support for general-purpose mounting and display assembly tasks.
Product Key Features
- Rubber adhesive delivers quick “grab” for fast bonding
- Provides light conformability and consistent thickness
- Adhesive on both sides for easy mounting and joining
- Ideal for lower-performance, general-purpose applications
- Suitable for temporary or non-structural uses
- Works with paper, plastics, films, and lightweight components
Applications
- Assembly of point-of-sale (POS) displays
- Mounting posters and display items
- Bonding lightweight nameplates and emblems
- Manufacturing sample cards
- Splicing paper, foil, and film
- General light-duty mounting and joining tasks
Packaging
Unit of measure Roll
Net weight 0.391812 kg
Gross weight 0.391812 kg
Dimensions 15 x 15 x 8 cm