3M™ Super 77™ Universal Spray Adhesive

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Super 77™ Universal Spray Adhesive

Main features

  • High tack
  • High coverage
  • Fast drying

Product Description

3M™ Super 77™ Multipurpose Spray Adhesive (Aerosol) is a high-performance, industrial-grade adhesive designed to deliver strong, permanent bonds with exceptional speed and efficiency. Featuring a high-tack, fast-drying formulation, this versatile spray adhesive provides excellent initial adhesion (“grab”) combined with a controlled open time, allowing for precise positioning before the bond fully sets.

This multipurpose adhesive is ideal for a wide range of applications, enabling reliable bonding of materials such as foils, carpeting, lightweight foams, paper, cardboard, felt, and cloth. It adheres effectively to various substrates including painted and unpainted metals, wood, hardboard, and other common base materials. Its transparent drying formula ensures clean, professional-looking results without compromising the appearance of bonded surfaces.

Designed for consistent performance, 3M™ Super 77™ delivers high coverage with minimal overspray and low soak-in characteristics, resulting in stronger, more uniform bonds and improved material finish. Whether used in manufacturing, maintenance, or general-purpose applications, it provides a dependable solution for fast-paced environments that demand both strength and efficiency.

Product Key Features

  • High-tack, fast-drying adhesive for strong, permanent bonds
  • Multipurpose formula suitable for a wide variety of materials and surfaces
  • Bonds foils, carpeting, lightweight foams, paper, cardboard, felt, and cloth
  • Adheres to painted/unpainted metals, wood, hardboard, and other substrates
  • Provides strong initial “grab” with sufficient open time for repositioning
  • Transparent drying for clean, professional results
  • Low soak-in formulation enhances bond appearance and increases coverage
  • Ideal for industrial, maintenance, and general-purpose bonding applications
Product Family

3M-77/CRM500ML

Cream, 500 ml
1. Select Package Type
2. Select Color

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Cartridge
Net weight 0.483 kg
Gross weight 0.483 kg
Dimensions 6.5 x 6.5 x 23.8 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry Type
Synthetic Elastomer
Color
The color
Translucent
Density
Volumetric mass per unit
720 kg/m3
Solids
25 %