3M™ Hot Melt Adhesive 3762LM

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M™ Hot Melt Adhesive 3762LM

Main features

  • 100% solids, no VOCs
  • Easy to use
  • Fast-setting adhesive obtains strength in seconds

Product Description

3M™ Hot Melt Adhesive 3762LM is a versatile, high-performance thermoplastic adhesive designed to deliver fast, efficient bonding for a wide range of lightweight materials. As a 100% solids, heat-applied adhesive, it contains no volatile organic compounds (VOCs), supporting cleaner operation and improved workplace efficiency.

Engineered with low melt (LM) characteristics, this adhesive is specifically formulated for low-temperature application, making it ideal for use on heat-sensitive substrates. Its low to medium viscosity allows for smooth flow and easy application, while its excellent “hot tack” provides instant adhesion upon contact. The adhesive quickly cools and solidifies into a strong, tack-free bond within seconds, eliminating the need for clamps or extended curing times.

Product Key Features

  • 100% solids formulation with no VOCs for cleaner operation
  • Low melt (LM) design for safe application on heat-sensitive substrates
  • Excellent “hot tack” for immediate bonding upon contact
  • Fast-setting adhesive achieves strength within seconds
  • “Quick grab” performance cools to a strong, tack-free bond
  • Low to medium viscosity for smooth, controlled application
  • Bonds a wide range of substrates including corrugated, beadboard, chipboard, wood, and lightweight materials
  • Easy to use and ideal for high-efficiency production environments
  • Well-suited for packaging, assembly, and woodworking applications
Product Family

3M-3762LM/BG5KG16X200

Beige, 16 mm x 200 mm, 5 kg
1. Select Package Type
2. Select Width
3. Select Length

Loading pricing…

Product availability
EU Shipping in 2 weeks
Packaging
Unit of measure Box
Net weight 5.364 kg
Gross weight 5.364 kg
Dimensions 27 x 16.8 x 21.6 cm
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Light Amber
Density (g)
1.01 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
293.3 °C